• Nickel alloy 230 Sheet Plate Haynes 230/UNS N06230 Sheet Plate
PRODUCT

MESSAGE

If you have any questions, please contact us and we will contact you as soon as possible.

Submit

Nickel alloy 230 Sheet Plate Haynes 230/UNS N06230 Sheet Plate

Nickel alloy 230 Sheet Plate Haynes 230/UNS N06230 Sheet Plate
Phone:+8617768786989
Email:simon@alloysfactory.com
WhatsApp:+8617768786989
Add:Room 412, Building 10, Fuqian Xingzuo Garden, Development Zone, Danyang City, Jiangsu Province
Inquire Now

◉ PRODUCT SPECIFICATION

Overview


Haynes 230 alloy is a nickel-chromium-tungsten-molybdenum alloy that combines excellent high-temperature strength, outstanding resistance to oxidizing environments up to 2100°F (1149°C) for prolonged exposures, premier resistance to nitriding environments, and excellent long-term thermal stability. It is readily fabricated and formed, and is castable. Other attractive features include lower thermal expansion characteristics than most high-temperature alloys, and a pronounced resistance to grain coarsening with prolonged exposure to high temperatures.


Limiting Chemical Composition, %

Nickel..............................................................................................................................................Balance

Carbon............................................................................................................................................0.05-0.15

Copper............................................................................................................................................20.0-24.0

Tungsten.....................................................................................................................................13.00-15.00

Cobalt.............................................................................................................................................5.00 max.

Molybdenum.......................................................................................................................................1.0-3.0

Aluminium.......................................................................................................................................0.20-0.50

Titanium..........................................................................................................................................0.10 max.

Iron...................................................................................................................................................3.00 max.

Lanthanum....................................................................................................................................0.005-0.05

Boron.............................................................................................................................................0.015 max.

Silicon..............................................................................................................................................0.25-0.75

Manganese......................................................................................................................................0.30-1.00

Sulphur...........................................................................................................................................0.015 max.

Copper..............................................................................................................................................0.50 max.

Phosphorus.....................................................................................................................................0.03 max.



Physical Constants


Density

lb/in^3.........................................................................0.324

g/cm^3..........................................................................8.96

Melting Range

°F...................................................................................2405

°C..................................................................................1343



Mechanical Properties


The mechanical properties of Haynes 230 alloy are excellent. It has a yield strength at a room temperature of 210 MPa and an ultimate tensile strength at a room temperature of 500 MPa. It also has good ductility with a strain hardening exponent of 0.15 and an elongation at a break of 20%.


Yield Strength,MPa

Tensile Strength,MPa

% Elongation in 2"

≥275

≥485

≥15



Corrosion Resistance


Haynes 230 alloy is highly resistant to corrosion in both acidic and alkaline environments, making it ideal for harsh environments where other alloys may not be suitable. It also has good oxidation resistance at elevated temperatures up to 1200°C, which makes it suitable for use in high-temperature applications such as aircraft turbine engines or industrial furnaces where other alloys may not be able to handle the heat load without deteriorating quickly.


Thermal Treatments:

Haynes 230 is a cobalt-based superalloy, and in order to optimize its properties, the following heat treatment steps are usually required:



Solution treatment: Haynes 230 is heated to 1150°C (2102°F) and held for 2 hours to ensure that the alloying elements are fully dissolved in the matrix.


Rapid cooling: After the solution treatment is completed, the material should be immediately air-cooled or water-cooled to room temperature to prevent alloying elements from precipitation during the cooling process.


Aging: Haynes 230 is heated to 870°C (1600°F) for 16 hours, then cooled to 760°C (1400°F) with the furnace, and finally air-cooled to room temperature. This step aims to precipitate alloying elements in the matrix and enhance the properties of the material.

Available  Forms


We provide you with a variety of product forms, including but not limited to.



● Bars & Rods

● Strips & Tape

● Wire & Welding

● Pipe & Tube

● Sheet & Foils

● Flanges & Forgins


Factory Show

  • O23
  • O38
  • O81
  • 摄图网_600752336_钢铁烈焰浇铸(非企业商用)

◉ MESSAGE

Submit

◉ SIMILAR RECOMMENDED